1K107 E-Shape Nanocrystalline Cores for Switching Power Supplies

Oct 27, 2025

Leave a message

What Is a 1K107 E-Shape Nanocrystalline Core?

The 1K107 designation refers to an iron-based nanocrystalline soft magnetic alloy with very high permeability, high saturation flux density and low core loss at high frequency. When manufactured in an E-shape, the core provides a convenient three-limb magnetic structure that is easy to wind and to mount on a PCB or chassis. E-shape nanocrystalline cores are used in switching power supply units to improve performance, particularly in high-power, high-frequency applications such as inverters, battery chargers and industrial equipment, where they deliver a more compact and efficient design than conventional ferrite cores.

Key Benefits Compared with Ferrite

High saturation magnetic induction: the 1K107 alloy saturates at about 1.2 T, roughly 2.5 times the saturation flux density of power ferrite, allowing smaller transformers with higher power density or a larger flux swing for the same core size.

Low core loss at high frequency: nanocrystalline cores have significantly lower core losses at 20-50 kHz than ferrite, increasing efficiency and reducing heat generation in the transformer.

Excellent thermal stability: with a Curie temperature around 570 °C, the magnetic performance stays stable over a much wider temperature range than ferrite, whose properties degrade well below 200 °C.

Compact design: the superior magnetic properties allow smaller core sizes, which is critical for applications with limited space such as vehicles, chargers and medical equipment.

High permeability: the high initial permeability reduces the number of turns required for a given inductance, lowering copper loss and winding cost.

Applications in Switching Power Supplies

Main transformers

Large switching power supplies and inverters use E-shape nanocrystalline cores for their main transformers to handle high power efficiently. The high saturation flux allows a smaller core cross-section, while the low loss keeps the temperature rise within limits at high switching frequencies.

High-frequency transformers

For forward, flyback and LLC resonant converters operating at 20-100 kHz, the low core loss of nanocrystalline material is a decisive advantage. The transformer can operate with a higher flux swing, reducing the number of turns and the copper loss.

Inductors and chokes

E-shape nanocrystalline cores are used in common-mode inductors, PFC (power factor correction) inductors and filtering inductors. In PFC boost inductors, the high saturation flux density and the option of a controlled air gap allow high energy storage in a small volume.

Other power electronics

Additional applications include UPS systems, solar power inverters and IGBT inverter power supplies, where efficiency, thermal stability and compactness are equally important.

Typical Dimensions

The table below lists representative E-shape nanocrystalline core dimensions. A, B, C, D, E and F are the standard E-core geometry parameters; tolerance values are given after the plus-minus sign.

A (mm) B (mm) C (mm) D (mm) E (mm) F (mm)
8.3 ± 0.2 6.0 ± 0.1 1.8 ± 0.2 3.6 ± 0.2 3.0 ± 0.1 4.0 ± 0.1
10.0 ± 0.3 7.0 ± 0.2 2.4 ± 0.2 4.6 ± 0.3 4.2 ± 0.2 5.4 ± 0.2
13.0 ± 0.3 10.2 ± 0.3 2.6 ± 0.2 5.9 ± 0.2 4.6 ± 0.1 6.0 ± 0.2
16.0 ± 0.3 12.0 ± 0.3 3.8 ± 0.2 4.8 ± 0.2 5.2 ± 0.2 7.2 ± 0.1
19.0 ± 0.3 14.0 ± 0.2 4.8 ± 0.3 4.8 ± 0.3 5.7 ± 0.2 8.0 ± 0.3
22.0 ± 0.6 15.6 ± 0.2 5.7 ± 0.3 5.7 ± 0.3 5.4 ± 0.3 9.2 ± 0.3
25.0 ± 0.4 18.6 ± 0.3 6.5 ± 0.3 6.5 ± 0.3 6.8 ± 0.2 10.0 ± 0.2
28.0 ± 0.6 18.6 ± 0.3 7.2 ± 0.2 10.7 ± 0.3 6.5 ± 0.2 10.5 ± 0.3
30.0 ± 0.5 19.9 ± 0.4 6.9 ± 0.3 7.1 ± 0.2 10.0 ± 0.2 15.0 ± 0.2
33.0 ± 0.3 23.5 ± 0.3 9.6 ± 0.4 12.7 ± 0.3 9.2 ± 0.3 13.7 ± 0.3
35.0 ± 0.6 24.6 ± 0.2 10.0 ± 0.3 10.0 ± 0.3 12.5 ± 0.3 17.5 ± 0.3
42.1 ± 0.9 29.5 ± 0.2 12.0 ± 0.3 15.0 ± 0.3 15.2 ± 0.4 21.1 ± 0.3

The dimensions above are for reference. Additional sizes and geometries can be customized to meet specific power and space requirements, including gapped versions for energy-storage inductors.

Design Considerations for the Power Supply Engineer

Verify the flux swing: nanocrystalline cores allow a larger delta-B than ferrite, but the core loss increases rapidly with frequency and flux density, so check the loss curve at the actual operating point.

Consider the air gap: for PFC and filter inductors, a controlled gap is needed to store energy; for transformer applications, an ungapped core maximizes permeability and minimizes magnetizing current.

Check the winding window: the E-shape window area and the core cross-section together determine the achievable power. Use the A x B product of the core to estimate the power capability in the first design pass.

Temperature derating: although the Curie temperature is high, the wire insulation and the core coating set the practical temperature limit; keep the core temperature below about 120-150 °C for long-term reliability.

Handling: nanocrystalline cores are sensitive to mechanical stress. Use the supplied protective coating and avoid clamping the core directly on its magnetic path.

FAQ

What does 1K107 mean in the core designation?

1K107 is the grade designation of the iron-based nanocrystalline alloy: it identifies the specific composition and heat treatment that give the core its high permeability, high saturation flux density and low core loss. Different grades in the 1K series are optimized for different combinations of loss, permeability and frequency range.

Why is the saturation flux density important in a switching power supply transformer?

A higher saturation flux density allows the transformer to operate with a larger flux swing, which means fewer turns and a smaller core for the same power. With ferrite, the usable flux swing is limited to about 0.2-0.3 T, while nanocrystalline material can operate at 0.5-0.8 T or more, roughly halving the core cross-section for the same power.

Can E-shape nanocrystalline cores be used at frequencies above 100 kHz?

They can, but core loss increases with frequency, so the flux swing must be reduced accordingly. Between 20 and 100 kHz the material offers a clear advantage over ferrite; above 100-200 kHz, the comparison depends on the specific alloy grade and the required efficiency.

How does a nanocrystalline E-core compare with a ferrite E-core of the same size?

For the same geometry, the nanocrystalline core provides roughly 2.5 times the saturation flux density and lower core loss at 20-50 kHz, enabling higher power throughput. The ferrite core is lighter, cheaper and easier to obtain in very large sizes, so the choice depends on the power density, cost and thermal requirements of the design.

Do nanocrystalline cores need an air gap for PFC inductors?

Yes. Energy-storage inductors such as PFC boost inductors require an air gap to store energy in the magnetic field. The core can be supplied with a distributed gap or a discrete gap so that the inductance remains stable under DC bias without saturating.