Silicon Steel C-Cut Cores (CD Type): Grain-Oriented Cut Cores for 50 Hz and 400 Hz Transformers
Sep 30, 2025
Leave a message
What a Silicon Steel C-Cut Core Is
A C-cut core is made by winding a thin strip of silicon steel into a ring, bonding or banding the wound body, and then cutting the ring into two C-shaped halves. Together the two halves close the magnetic circuit; separated, they let a pre-wound bobbin or former be slipped onto the limb before the halves are clamped together again. The cut faces are usually ground flat so that the two halves mate with a very small residual gap. This geometry is used wherever a closed, gapless winding operation is impractical - for example with heavy magnet wire, with multiple windings, or with a bobbin that must be fitted after the core has been annealed.
Two related product families share the same manufacturing route: the true C-cut core, which is a cut ring with circular or oval windows, and the UU core, which is formed from two U-shaped halves in the same way. Both deliver the key advantage of wound cores - the flux always follows the rolling direction of grain-oriented strip - while allowing assembly around a finished coil.
Materials, Grades and Thickness Options
Core material - cold-rolled grain-oriented silicon steel for low loss along one axis, or cold-rolled non-oriented silicon steel where flux paths are mixed or cost dominates.
Grain-oriented grades - 23ZH85, 23ZH105, 27ZH105, 30ZH120 and similar designations, in which the numeric suffix indicates the nominal maximum specific total loss in W/kg measured at 1.7 T and 50 Hz: 23ZH85 is about 0.85 W/kg, 27ZH105 about 1.05 W/kg and 30ZH120 about 1.20 W/kg.
Non-oriented grades - strip such as the H500 class, whose specific loss is specified at 1.5 T and 50 Hz, used for economical 50 Hz cores and for mixed flux paths.
Strip thickness - 0.23 mm, 0.27 mm, 0.30 mm and 0.35 mm are the standard options for grain-oriented material; thinner strip reduces eddy-current loss and is the natural choice as frequency rises.
Finish - the core can be supplied as an impregnated bare core or with an epoxy resin coating for mechanical protection and improved insulation to the coil.
Saturation induction of grain-oriented silicon steel is about 2.0 T, with working flux densities typically 1.5-1.7 T, so the practical advantage of this material is not higher saturation but lower loss and higher permeability in the rolling direction.
Features and Performance Characteristics
Low loss and high initial permeability - the wound strip follows one continuous rolling direction, so specific loss at 50 Hz approaches the best value the grade can deliver.
Excellent DC bias behaviour - the deliberate cut introduces a small controlled gap, and the resulting sheared B-H loop lets the core carry a DC component without saturating, which matters in rectifier and filter inductors.
Easy coil assembly - the two halves separate completely, so bobbins can be machine wound and then dropped into place.
Stable, reproducible gap - the mating faces are ground flat and the two halves are clamped by the mounting frame, so the assembled gap is typically in the order of 0.02-0.05 mm and can be adjusted with thin insulating shims when a defined inductance is required.
Mechanical robustness - banding or impregnation holds the cut ends in alignment, and the epoxy option adds protection against humidity and handling damage.
Standard CD Sizes and Ratings
The CD series is designated by the window width a, the strip width b and the stack height h, all in millimetres. The table gives representative members of the range with their core weight and apparent power rating at 50 Hz and 400 Hz; the 400 Hz figures rise sharply because the same core can transfer far more volt-amperes before the loss limit is reached, even after allowing for the increase in core loss with frequency.
| Model | a x b x h (mm) | Weight (kg) | Rating at 50 Hz (VA) | Weight (kg) | Rating at 400 Hz (VA) |
|---|---|---|---|---|---|
| CD10x12.5x20 | 10 x 12.5 x 20 | 0.091 | 1.85 | 0.088 | 52 |
| CD12.5x16x25 | 12.5 x 16 x 25 | 0.185 | 8.5 | 0.178 | 106 |
| CD16x32x40 | 16 x 32 x 40 | 0.705 | 77.1 | 0.682 | 427 |
| CD20x40x50 | 20 x 40 x 50 | 1.386 | 174 | 1.342 | 740 |
| CD25x50x65 | 25 x 50 x 65 | 2.761 | 396 | 2.673 | 1453 |
| CD32x64x80 | 32 x 64 x 80 | 5.665 | 906 | 5.478 | 2913 |
| CD40x80x100 | 40 x 80 x 100 | 11.11 | 1950 | 10.791 | 5608 |
The smaller members of the family have relatively thicker strip in proportion to the window and are used at low power; as the window grows, loss control and gap flatness become the limiting factors rather than the material grade.
Applications, Selection and Verification
C-cut and UU cores are used in 50 Hz to 400 Hz transformers, AC and DC reactors, smoothing and filter chokes, inductors, current transformers, magnetic amplifiers, voltage stabilisers and control components in electronic equipment. When selecting a core, start from the required volt-amperes and the working frequency: a 400 Hz design can use a much smaller core than a 50 Hz design for the same rating, but it benefits from thinner strip because eddy-current loss grows with frequency. Where a DC component is present, size the core for the bias requirement and rely on the controlled gap to keep the inductance predictable.
Verification of a delivered C-cut core should cover strip grade and thickness against the certificate, core weight and dimensions, window and limb tolerances, gap flatness of the cut faces, surface finish, and - on a sample basis - specific loss and exciting current. Because the winding is fitted to a cut core after the fact, close checking of the gap and of the clamping arrangement matters more than for a closed toroid: an unevenly clamped joint adds loss and audible noise that cannot be corrected later.
FAQ
Q: What is the difference between a C-cut core and a toroidal core?
A toroidal core is never cut and therefore has no joints and the lowest loss, but the winding must be threaded through the window. A C-cut core trades a small joint loss for the ability to fit a pre-wound coil onto the limb.
Q: Why cut the core instead of winding it closed?
Because practical coils - heavy wire, multiple secondaries, bobbins with terminals - often cannot be wound through a closed window, and because the cut halves let the core be annealed and coated before the coil is assembled, avoiding damage to the winding from heat treatment.
Q: How large is the gap and how is it controlled?
The cut faces are ground flat and clamped, giving a residual gap typically in the order of 0.02-0.05 mm. Where a defined gap is required for DC bias or for a specific inductance, insulating shims of known thickness are inserted between the mating faces.
Q: Which grade suits 400 Hz operation?
Grain-oriented grades with the thinnest strip available, since eddy-current loss rises with frequency and declines with the square of thickness. The 23ZH85 and 23ZH105 grades are typical; thicker 30ZH120 strip is generally reserved for 50 Hz work.
Q: What does the VA figure in the CD table mean?
It is the apparent power the core can handle at the stated frequency within a defined loss and temperature-rise limit. Because 400 Hz cores are limited by core loss rather than by saturation, the same core shows a much higher VA rating at 400 Hz.