What Are Nanocrystalline Block Cores?

Nanocrystalline block cores are rectangular soft magnetic components manufactured from 1K107 iron-based nanocrystalline alloy. The material is produced by rapidly solidifying a melt into thin ribbon, then annealing it under a controlled magnetic field so that a fine grain structure with an average grain size of 10 to 20 nm forms. Block cores are built by stacking and bonding ribbon segments or by winding ribbon into rectangular shapes, which gives a large effective cross-section and a compact magnetic circuit for high-power equipment.

Key Magnetic Properties of 1K107 Block Cores

The following table summarizes the typical magnetic properties of 1K107 nanocrystalline block cores. Values are measured under standard laboratory conditions and may vary with core dimensions, assembly shape and air-gap length.

Property Typical value
Saturation flux density Bs 1.23 T
Saturation magnetostriction λs <1 ppm
Core loss P 0.4 W/kg at 10 kHz, 0.1 T
Curie temperature Tc 570 °C
Effective relative permeability µre 5,000 at 10 kHz
Maximum operating temperature 130 °C

Magnetic parameters are characterized in accordance with GB/T 19346.1 and IEC 60205, which define the measurement methods and the calculation of effective core parameters.

Why Block Cores for High-Power Medium-Frequency Transformers

Medium-frequency transformers for high-power capacity typically operate between several hundred hertz and tens of kilohertz. At these frequencies, conventional grain-oriented silicon steel suffers from high eddy-current loss, while ferrite lacks the saturation flux density needed to handle high power in a compact volume. 1K107 nanocrystalline block cores combine a saturation flux density of 1.23 T with core loss of only 0.4 W/kg at 10 kHz and 0.1 T, allowing the transformer designer to reduce both core size and temperature rise.

The near-zero magnetostriction of 1K107 also keeps audible noise low, which matters for railway auxiliary supplies, inverters and other installations where acoustic limits are specified. A high effective permeability around 5,000 at 10 kHz keeps the magnetizing current low and simplifies winding design.

Typical Applications

Inverters for alternative energy and auxiliary power supplies for trains

Quick chargers for electric vehicles and isolated DC/DC converters

Reactors for photovoltaic inverters

Filter reactors for high-frequency switching power supplies

Selection and Design Considerations

When selecting a nanocrystalline block core, verify the operating frequency, the peak flux density and the allowable temperature rise together. Because effective permeability depends on core geometry and any air gap in the assembly, request the effective parameters (Ae, Ie, Le) for the exact core size from the manufacturer. GNEE New Material supplies 1K107 block cores in a range of cross-sections and window dimensions, and can provide measured core-loss data for the specific assembly rather than typical values only.

FAQ

1. What is the difference between a block core and a toroidal core?

A block core has a rectangular magnetic path and is normally assembled from stacked or wound ribbon segments, which suits large cross-sections and easier winding of heavy copper coils. A toroidal core is wound as a continuous ring and gives a fully closed magnetic circuit with minimum leakage, but winding a toroid requires a shuttle and is more difficult for thick wire.

2. Why is 1K107 preferred for medium-frequency transformers?

1K107 offers a balanced combination of high saturation flux density (1.23 T), low core loss at 10 kHz and above, low magnetostriction and good thermal stability up to 130 °C, which matches the requirements of high-power medium-frequency magnetic components.

3. Can block cores be gapped for DC bias applications?

Yes. A controlled air gap can be introduced during assembly to raise the tolerance to DC bias in reactor and inductor applications. Note that the gap reduces effective permeability, so the inductance calculation must be revised using the effective magnetic path length.

4. What standards apply to the measurement of these cores?

Core-loss and permeability measurements follow GB/T 19346.1 and IEC 60205. Transformers built with these cores are normally designed and tested to the IEC 60076 series where applicable.

5. How should 1K107 block cores be handled and stored?

Cores are shipped with an insulation coating. Avoid mechanical shock that can crack the ribbon edges, keep cores dry and store them away from strong magnetic fields. Mechanical stress after annealing degrades soft magnetic properties, so treat cores as finished precision components.

Send Inquiry