How to Heat Treat Electrical Steel?
Nov 24, 2023
Leave a message
GNEE New Material Electrical Steel Sheet
Heat treatment process is one of the important technologies in the processing of electrical steel. The heat treatment process has a great influence on the magnetic properties of electrical steel products. Electrical steel is actually an iron-silicon alloy. The heat treatment of electrical steel is a discipline that studies the relationship between the properties of electrical steel and the heating temperature, time and atmosphere of the furnace and cold zone. Therefore, it can be said that the heat treatment of electrical steel is a process in which the organizational structure of electrical steel is changed under the action of heating, insulation, cooling and atmosphere in the furnace to obtain the required properties.
In addition to the normal annealing of hot-rolled coils, cold-rolled electrical steel strips also need to undergo various forms of heat treatment after cold rolling. Intermediate decarburization annealing, work hardening elimination annealing, magnesium oxide isolation layer drying treatment, high-temperature round furnace And shield furnace annealing, stretch heat leveling annealing, finished product annealing and insulation layer drying and sintering treatment.
Most of the soft magnetic materials used at the end of the 19th century were industrial pure iron. Adding a small amount of silicon to the iron core's iron loss can improve the magnetic induction and greatly reduce the iron loss. Research has found that silicon plays a decisive role in the level of magnetic induction. This is because: the value is very large, the magnetic induction is below 10,000 Gauss, and the magnetic loss value is 3-6W/kg. As a result, generators, motors, and transformers are produced that are large, poor quality, and inefficient. Later, it was discovered that adding a small amount of silicon can improve the magnetic induction and greatly reduce the iron loss. Research has found that silicon plays a decisive role in the level of magnetic induction because: silicon can increase magnetic permeability, reduce coercive force, and reduce hysteresis loss; at the same time, silicon can also promote graphitization of carbon and reduce the impact of carbon on magnetism. harmful effects. Due to the above-mentioned effects of silicon, ferroelectric alloys are now widely used in electric motors, transformers and communications industries. The commonly used electrical steel sheets are Fe-Si binary alloys with few other impurities.
Silicon steel coil

Therefore, as the amount of Si increases, the iron loss decreases and the magnetic sensitivity increases, but the brittleness increases, making it difficult to process and form. Generally, the silicon content of silicon-free electrical steel is less than 0.3%, the silicon content of low silicon electrical steel is within 0.3-0.8%, the silicon content of medium electrical steel is within 0.8-2.4%, and the silicon content of high electrical steel is within 0.3-0.8%. Within 2.5-3.4%.
Silicon has a great influence on the properties of iron-silicon alloys. Even a small amount of silicon can significantly change the physical and mechanical properties of iron-silicon alloys. Adding silicon to iron can increase the hardness and strength, while reducing the elongation and impact toughness. Silicon is particularly sensitive to brittleness, making processing difficult.
The Si content of cold-rolled electrical steel sheets is generally below 3.5%. The higher the Si content, the greater the brittleness and the more difficult it is to roll and form. The Si content of hot-rolled electrical steel sheets is generally less than 5%. This is because the plasticity of Fe-Si alloys is closely related to temperature. For example, electrical steel with a Si content of 4.5% is very brittle at room temperature, but can be rolled when heated to about 100°C. When producing electrical steel sheets, in the final annealing of the magnetic gap, if the temperature range of the γ phase is annealed, the magnetic properties will become worse. Cold-rolled non-oriented electrical steel sheets rely on the continuous annealing time to make them magnetic, but the higher the silicon content of the electrical steel, the stronger the ability to anneal at high temperatures, so the oriented electrical steel sheets rely on high temperatures in a ring furnace or shielded furnace. Annealing for a long time makes it magnetic, so the silicon content of grain-oriented electrical steel must be greater than 2.5%.
Cold Rolled Electrical Steel