Applications of Non-Oriented Silicon Steel in Motors, Transformers and Generators

Oct 20, 2025

Leave a message

What Non-Oriented Silicon Steel Is

Non-oriented silicon steel, also called non-grain-oriented electrical steel, is a flat-rolled iron-silicon alloy whose crystal grains have no preferred orientation. Because the grains point in all directions, magnetic properties such as permeability and core loss are essentially uniform in the rolling direction and across it, which is exactly what a rotating machine needs. Typical silicon content is between 0.5 percent and 3.5 percent, with aluminium and manganese added in small amounts to control resistivity and grain growth, and carbon, sulphur and nitrogen held to low levels to avoid magnetic ageing.

Silicon is added for two reasons. It raises electrical resistivity, which reduces eddy-current loss, and it lowers magnetocrystalline anisotropy and magnetostriction, which reduces hysteresis loss and acoustic noise. The penalty is that higher silicon makes the strip harder and more brittle, so very high silicon grades are difficult to punch and are reserved for applications where the loss saving justifies the tooling cost.

Magnetic Characteristics

Three quantities describe most purchasing decisions: specific total loss in watts per kilogram at a stated flux density and frequency, magnetic induction at a stated field strength, and stacking factor. Core loss falls as thickness decreases, because eddy-current loss scales roughly with the square of thickness, so 0.35 mm and 0.50 mm stock is common for rotating machines while 0.20 mm to 0.27 mm grades are used for high-frequency machines and for stators that run at high pole counts.

Parameter Typical non-oriented range Effect on design
Silicon content 0.5 % to 3.5 % resistivity up, loss down, punchability down
Thickness 0.20 mm to 0.65 mm eddy-current loss falls with thickness squared
Specific total loss quoted in W/kg at 1.5 T and 50 Hz directly sets stator and rotor heating
Stacking factor typically about 0.95 to 0.98 determines effective iron length in the stack
Anisotropy nearly isotropic in the plane of the sheet essential for rotating machines

Grade designations encode thickness and loss: the first two digits give the nominal thickness in hundredths of a millimetre, and the following digits give the maximum specific total loss in watts per kilogram multiplied by a hundred, measured at the reference flux density and frequency of the applicable specification. Grade requirements for non-oriented electrical steel strip and sheet are set out in IEC 60404-8-4 and EN 10106, with ASTM A677 covering fully processed non-oriented types. Loss and induction are measured by Epstein frame under IEC 60404-2 or by single sheet tester under IEC 60404-3.

Production Route

The conventional route is melting, continuous casting, hot rolling, pickling, cold rolling and continuous annealing. In the fully processed condition the strip is delivered with the recrystallisation anneal and the insulating coating already applied, so the user punches, stacks and welds without a further anneal. In the semi-processed condition the strip is delivered with a controlled carbon level, and the user performs a decarburising anneal after punching; this is common for small motor laminations where the punching operation would otherwise degrade the magnetic properties along the cut edge.

Coating choice matters as much as the steel. A thin organic or inorganic coating provides interlaminar insulation and also affects punchability, weldability and stacking factor. Where the machine is impregnated with varnish, the coating must be compatible with the resin, otherwise the stack can delaminate or the insulation resistance between laminations can fall.

Applications

Non-oriented silicon steel is used wherever the magnetic flux path rotates or where low cost outweighs the directional advantage of grain-oriented material:

Induction motors and generators - stators and rotors of industrial drives, pumps, fans and compressors, generally in 0.35 mm or 0.50 mm thickness.

Small and medium power transformers - distribution transformers below the size where grain-oriented steel pays back, and instrument transformers.

Ballasts, reactors and chokes - laminated magnetic components in lighting and power electronics.

Compressors, appliances and hermetic motors - high-volume punching applications that need consistent properties and good punching life.

Electric vehicle traction motors - thin, high-frequency grades where loss at several hundred hertz matters more than peak induction.

Selection logic follows the excitation. If the flux direction is fixed and the material can be oriented, grain-oriented steel gives lower loss at line frequency. If the flux rotates, or if the part is small and punching dominates cost, non-oriented steel is the correct choice. In variable-speed drives the excitation frequency is much higher than line frequency, and thinner non-oriented grades with lower loss at 400 Hz often beat thicker grades on total loss.

Quality and Handling Notes

Loss is sensitive to mechanical stress. Punching, shearing and even tight winding of a coil raise loss, and this effect is larger in the region within a few millimetres of a cut edge. Good practice is therefore to keep the cut edges out of the highest-flux region where possible, to avoid excessive clamping pressure, and to specify an annealing treatment when the design is loss-critical. Stacking factor and burr height should be specified together, because a large burr both shorts laminations and reduces the effective iron length. Finally, because test data is measured on the Epstein specimen with the field in the rolling direction, the loss of a real stator will be higher, so margins of at least 10 to 20 percent are normal in machine design.

Frequently Asked Questions

Q: What is the difference between non-oriented and grain-oriented silicon steel?
A: Grain-oriented steel is processed so that the crystals align with the rolling direction, giving very low loss along that direction but poor properties across it, while non-oriented steel stays nearly isotropic and is therefore used in motors and generators.

Q: How much silicon is in non-oriented silicon steel?
A: Typically 0.5 percent to 3.5 percent by weight, with common motor grades around 1 percent to 2.5 percent, since higher silicon lowers loss but makes the strip harder to punch.

Q: What thickness should be selected for a 400 Hz motor?
A: Thinner stock, generally 0.20 mm to 0.35 mm, is preferred above line frequency because eddy-current loss rises with the square of thickness, and total loss at the higher frequency usually decides the choice.

Q: Which standards apply to non-oriented electrical steel?
A: Grade requirements are given in IEC 60404-8-4 and EN 10106, with ASTM A677 covering fully processed non-oriented types, while loss and induction are measured by Epstein frame per IEC 60404-2 or by single sheet tester per IEC 60404-3.

Q: Why does core loss rise after punching?
A: Shearing introduces plastic strain and dislocations along the cut edge, which increases hysteresis loss and can short neighbouring laminations if the burr is large; the effect is greatest within a few millimetres of the edge.

Q: Is a stress relief anneal always needed?
A: No. Fully processed material is annealed by the supplier and usually needs no further treatment, while semi-processed material requires a decarburising anneal after punching to develop its specified loss and induction.

Send Inquiry