Amorphous Multiple Air Gap C-Core: Design, Performance and Applications
Sep 30, 2025
Leave a message
What Is an Amorphous Multiple Air Gap C-Core?
An amorphous multiple air gap C-core is a rectangular C-shaped magnetic core built from rapidly solidified Fe-based amorphous alloy ribbon. The ribbon is wound, annealed, cut and then separated into several segments so that engineered air gaps are distributed along the magnetic path instead of being concentrated in one single cut. This structure gives designers precise control over the effective permeability of the core, which is the key to stable inductance under DC bias conditions.
The amorphous material is produced by quenching a molten Fe-Si-B alloy at a cooling rate above one million kelvin per second, which freezes the metal into a non-crystalline ribbon about 20 to 30 micrometers thick. Because there is no grain structure, the hysteresis loss is very small, and the ribbon can be stacked with a high lamination factor. Grade 1k101 is a standard Fe-based amorphous grade used for power magnetics in the 1 kHz to 100 kHz range.
Why Multiple Air Gaps Matter
A conventional single-gap C-core concentrates the entire air gap at one cut. Under high DC current the fringing flux around that single gap saturates the local core material, raises the hotspot temperature and produces audible noise. A multiple air gap design divides the gap into several shorter segments, which reduces the fringing flux density at each gap, lowers the temperature rise and improves the DC-bias characteristics of the choke.
Multiple gaps also reduce the mechanical vibration caused by magnetostriction and by magnetic attraction between the core halves. For switched-mode power supply output chokes and PFC boost chokes, this translates into quieter operation and a more linear inductance curve from no load to full load.
Material and Performance Data
The core is made from Fe-based amorphous alloy grade 1k101 with the following typical magnetic and physical properties:
| Parameter | Value |
|---|---|
| Saturation flux density Bs | 1.56 T |
| Hardness Hv | 960 kg/mm2 |
| Curie temperature Tc | 410 C |
| Electrical resistivity | 130 uOhm.cm |
| Crystallization temperature Tx | 500 C |
| Density | 7.18 g/cm3 |
| Magnetostriction lambda-s | 27 x 10-6 |
| Core loss Ps at 16 kHz, 37 mT | below 1.0 W/kg |
The high resistivity of 130 uOhm.cm, roughly three times that of grain-oriented silicon steel, suppresses eddy current losses at high frequency, while the 1.56 T saturation flux density allows a smaller core volume for a given rated current.
Typical Applications
Output smooth filter chokes for switched-mode power supplies
PFC boost chokes for solar inverters and EV charging piles
AC inverter chokes for PV inverters and active power filters
DC chokes and filter inductors in robotic systems
Line and load chokes in frequency converters
In all of these circuits the choke must carry a significant DC or low-frequency AC component while maintaining a defined inductance, which is exactly the condition where amorphous multiple air gap cores outperform silicon steel and ferrite alternatives.
Standard Dimension Range
The core is supplied as two matched C halves. The table below lists representative standard sizes; the notation follows a, b, c, d, e, f as the main window and outer dimensions, lm the mean magnetic path length, Ac the effective cross-section, Wa the window area, WaAc the area product and Mass the weight of one complete core.
| a mm | b mm | c mm | d mm | e mm | f mm | lm cm | Ac cm2 | Wa cm2 | WaAc cm4 | Mass g |
|---|---|---|---|---|---|---|---|---|---|---|
| 9 +/-0.5 | 10 | 32.8 | 15 +/-0.5 | 28 +/-1.5 | 50.8 +/-1.5 | 11.2 | 1.2 | 3.3 | 3.9 | 97 |
| 10 +/-0.5 | 11 | 33 | 20 +/-0.5 | 31 +/-1 | 53 +/-2 | 11.8 | 1.74 | 3.6 | 6.3 | 150 |
| 11 +/-0.8 | 13 | 40 | 25 +/-0.5 | 35 +/-1 | 62 +/-2 | 13.7 | 2.4 | 5.2 | 12.5 | 241 |
| 13 +/-0.8 | 15 | 56 | 30 +/-0.5 | 41 +/-1 | 82 +/-2 | 17.9 | 3.4 | 8.4 | 28.6 | 450 |
| 16 +/-1 | 20 | 70 | 30 +/-0.5 | 52 +/-1 | 102 +/-3 | 22.7 | 4.19 | 14 | 58.6 | 740 |
| 19 +/-1 | 25 | 83 | 40 +/-1 | 63 +/-1 | 121 +/-3 | 27.2 | 6.63 | 20.8 | 137.5 | 1321 |
| 22 +/-1 | 35 | 85 | 50 +/-1 | 79 +/-1 | 129 +/-3 | 30.4 | 9.59 | 29.8 | 285.4 | 2135 |
| 26 +/-1 | 45 | 88 | 40 +/-1 | 97 +/-1 | 140 +/-3 | 34.3 | 9.07 | 39.6 | 359.1 | 2275 |
| 30 +/-1 | 40 | 95 | 85 +/-1 | 100 +/-1 | 155 +/-4 | 35.7 | 22.24 | 38 | 845 | 5820 |
| 33 +/-1 | 40 | 105 | 85 +/-1 | 106 +/-1 | 171 +/-4 | 38.7 | 24.46 | 42 | 1027.3 | 6930 |
Custom sizes, air gap lengths and gapped segment counts can be produced to match the target inductance and DC current of a specific design.
Selection Notes and Common Mistakes
Determine the DC bias current and the required inductance at that current, not just the no-load inductance, because the effective permeability drops as DC current rises.
Check the temperature rise at the maximum ambient temperature; amorphous cores run hotter than ferrite at the same flux swing unless the gap distribution and copper losses are balanced.
Do not substitute a single-gap core of the same area product; the DC-bias and noise performance will differ significantly.
Verify the winding window before ordering; the area product WaAc is the quickest indicator of whether the required number of turns fits.
FAQ
What does multiple air gap mean in an amorphous C-core?
It means the magnetic path is divided into several small gaps instead of one large cut. Each gap segment limits fringing flux, which improves DC-bias stability, lowers temperature rise and reduces audible noise in high-current chokes.
Why use amorphous alloy instead of silicon steel for high-frequency chokes?
Amorphous alloy has roughly three times the electrical resistivity of silicon steel and very low hysteresis loss, so eddy current and hysteresis losses stay low at switching frequencies from 1 kHz to 100 kHz. This allows a smaller core volume and cooler operation.
What is the saturation flux density of 1k101 amorphous alloy?
The typical saturation flux density Bs is 1.56 T, which is higher than ferrite and sufficient for most power inductor designs while keeping the core volume compact.
How do multiple air gaps affect DC bias performance?
Distributed gaps spread the fringing flux and raise the effective saturation current, so the inductance remains more stable from light load to full load, which is essential for PFC boost and output filter chokes.
Which applications benefit most from this core design?
Switched-mode power supply output chokes, PFC boost chokes in solar inverters and EV charging piles, AC inverter chokes, active power filter reactors and frequency converter line chokes all benefit from the low loss and stable DC-bias behaviour.
Can the core dimensions be customized?
Yes. Core geometry, air gap length, number of gap segments and the winding window can be adjusted to meet a specific inductance, current rating and thermal budget.