Customized CRGO Electrical Silicon Steel Sheet for Transformer Cores
Oct 21, 2025
Leave a message
CRGO electrical silicon steel sheet is the cold rolled grain oriented material specified for transformer iron cores when high permeability and low core loss have to be held at the same time. The sheet is rolled so that its grains line up with the rolling direction, and that orientation is what allows a customized core to run cool at full load and draw very little exciting current at no load.
Because every transformer design has its own window, stack height and joint pattern, the sheet is normally supplied customized: slit to width, cut to length, punched to profile, or delivered as a finished assembled core. This article sets out the electrical grades available, the manufacturing route behind them and the dimensional options that can be specified.
What Defines CRGO Electrical Steel
Cold rolled grain oriented steel combines three deliberate features in one material:
Silicon content of roughly 2.9–3.3 % by mass, which raises electrical resistivity and holds eddy current loss down.
A Goss type grain texture produced by heavy cold reduction and secondary recrystallization, giving the sheet its strongly anisotropic magnetic behaviour.
A thin insulating coating, normally phosphate or oxide based, that keeps adjacent laminations electrically separated in the finished stack.
The practical consequence is that flux is carried efficiently along the rolling direction, so cores can be made smaller, lighter and cooler than an equivalent core built from non-oriented sheet.
Grades and Electrical Performance
The table below lists common grain oriented grades with their guaranteed loss class, lamination factor and minimum induction at 800 A/m. Core loss is quoted as specific total loss at 1.7 T and 50 Hz, and induction is quoted at a magnetizing field of 800 A/m.
| Grade | Width range | Max core loss at 1.7 T / 50 Hz | Lamination factor | Min induction at 800 A/m |
|---|---|---|---|---|
| 23Q110 | 35–1200 mm | 1.10 W/kg | 97.2 % | 1.82 T |
| 23Q120 | 35–1200 mm | 1.20 W/kg | 97.2 % | 1.82 T |
| 27Q120 | 35–1200 mm | 1.20 W/kg | 97.5 % | 1.82 T |
| 30G120 | 35–1200 mm | 1.20 W/kg | 98 % | 1.82 T |
High Induction and Domain Refined Options
Where a design calls for maximum flux density rather than minimum loss, high induction grades raise the induction level by about 0.06 T for the same thickness. Domain refined grades, produced by laser scribing, cut loss again while keeping the high induction level, and are chosen for large distribution transformers with tight no-load loss limits.
| Grade | Max core loss at 1.7 T / 50 Hz | Lamination factor | Min induction at 800 A/m |
|---|---|---|---|
| B20P085 | 0.85 W/kg | 97 % | 1.86 T |
| B23P085 | 0.85 W/kg | 97.2 % | 1.88 T |
| B23P090 | 0.90 W/kg | 97.2 % | 1.88 T |
| B23P095 | 0.95 W/kg | 97.2 % | 1.88 T |
| B23P100 | 1.00 W/kg | 97.2 % | 1.88 T |
| B27P095 | 0.95 W/kg | 97.5 % | 1.89 T |
| B27P100 | 1.00 W/kg | 97.5 % | 1.89 T |
| B30P120 | 1.20 W/kg | 98 % | 1.89 T |
| B20R070 | 0.70 W/kg | 97 % | 1.86 T |
| B23R085 | 0.85 W/kg | 97.2 % | 1.88 T |
| B27RK085 | 0.85 W/kg | 97.5 % | 1.89 T |
How the Sheet Is Made
Hot rolling - initial thickness reduction of the cast slab.
Cold rolling - further reduction carried out under precise thickness control.
Annealing - the critical step that develops the grain oriented structure.
Coating - an insulating layer, typically phosphate or oxide based, is applied to both faces.
Stress relief annealing - final heat treatment that stabilizes magnetic performance.
Customized Sheet and Core Specifications
Sheet is supplied cut to width from mill coil, and assembled cores can be built to drawing as either automatically or manually stacked constructions. Typical capability limits are summarized below.
| Item | Capability |
|---|---|
| Max weight, automatically stacked core | 60 ton |
| Max weight, manually stacked core | 120 ton |
| Gap limit at the joint | less than 1.0 mm |
| Window height precision | plus or minus 1 mm |
| Window width precision | plus or minus 1 mm |
| Sheet forms | slit strip, cut sheet, punched lamination, wound ring section |
CRGO sheet and assembled cores are used in distribution and transmission power transformers, instrument transformers, inductors, reactors and large electric motors and generators.
Frequently Asked Questions
Q: What does the letter Q in a grade such as 23Q110 mean?
Q identifies a conventional grain oriented grade. The leading digits give thickness in hundredths of a millimetre, so 23 means 0.23 mm, and the trailing digits give the loss class multiplied by 100, here 1.10 W/kg at 1.7 T and 50 Hz.
Q: How do high induction grades differ from conventional grades?
High induction grades, marked with a P, reach about 1.88 T at 800 A/m against 1.82 T for conventional grades, which allows a smaller core cross section for the same power rating.
Q: What is the benefit of domain refined sheet?
Laser scribing subdivides the magnetic domains, so loss falls sharply at the same induction. Grades marked with R are used where no-load loss limits are the deciding design constraint.
Q: Can cores be delivered fully assembled?
Yes. Both automatically stacked cores up to 60 ton and manually stacked cores up to 120 ton are built and clamped before shipment, with joint gap held below 1.0 mm and window dimensions to plus or minus 1 mm.
Q: How should CRGO sheet be stored before use?
Sheet should stay dry, flat and wrapped, away from impact and bending. Mechanical damage and moisture both raise core loss, and poor flatness reduces the achievable stacking factor.
Q: What information is needed to specify a customized core?
Grade, thickness, window height and width, stack height or core weight, joint type, coating requirement and the expected flux density and frequency of operation.