0.30 mm High Permeability Grain-Oriented Silicon Steel Slit Coil (30-120 mm)
Sep 26, 2025
Leave a message
Product Overview
Grain-oriented electrical steel (GOES) is the core material of efficient transformers and large generators. During production, a carefully controlled secondary recrystallisation grows grains of more than 30 mm in length, all aligned with the rolling direction. This orientation gives the steel outstanding magnetic properties in the rolling direction: low core loss, high permeability and high induction. The 0.30 mm high-permeability slit coil presented here is cut from full-width GOES coils into narrow strips of 30-120 mm width, ready for winding into toroidal cores, C-cores and other wound-core assemblies.
Why Grain Orientation Matters
In ordinary steel the magnetic domains are randomly arranged and the flux has to fight against misaligned grains. In grain-oriented steel the crystals are aligned so that the easy magnetisation direction coincides with the rolling direction. The flux path through a wound core follows this direction continuously, which minimises hysteresis loss and maximises permeability. The same physics is why transformer cores are always cut or wound so that flux runs along the rolling direction of the strip.
Key Characteristics
Magnetic Properties
The product features low core loss, high permeability and stable application performance. Loss is measured at 1.7 T and 50 Hz and expressed in W/kg, and induction is verified at a field strength of 800 A/m (B800).
Thickness Tolerance
Thickness is controlled in both the rolling and transverse directions, giving a high lamination factor so that more steel fits in the same core volume and the effective cross-section is maximised.
Processing Properties
The coated strip is suitable for punching, cutting and winding with excellent dimensional tolerance, allowing tight and consistent cores without burr damage to the insulation.
Insulation Coating
The coating has small colour deviation, good adhesion, high insulation resistance and good resistance to heating and corrosion. Several coating classes are available to suit different annealing and stress-relief processes.
Available Grades
GNEE New Material supplies conventional, high-induction and domain-refined (laser-scribed) grades in widths from 35 mm to 1200 mm. The high-induction types (B series) offer induction above 1.86 T at B800, while domain-refined types (R series) reach core-loss values as low as 0.70 W/kg at 1.7 T/50 Hz.
| Type | Grade | Width (mm) | Max Core Loss @1.7 T/50 Hz (W/kg) | Lamination Factor (%) | Min Induction @B800 (T) |
|---|---|---|---|---|---|
| Common | 23Q110 | 35-1200 | 1.10 | 97.2 | 1.82 |
| High induction | B23P090 | 35-1200 | 0.90 | 97.2 | 1.88 |
| High induction | B27P095 | 35-1200 | 0.95 | 97.5 | 1.89 |
| Domain refined | B23R085 | 35-1200 | 0.85 | 97.2 | 1.88 |
| Domain refined | B20R070 | 35-1200 | 0.70 | 97.0 | 1.86 |
Applications
Large and medium power transformers
Distribution transformers and pad-mounted units
Reactors and magnetic amplifiers
Current and potential transformers
Audio transformers, ballasts and welding transformers
Magnetic switch cores and wound-core assemblies
Processing and Handling
Slit coils must be stored horizontally on pallets in a dry warehouse to protect the coating and edges. During winding, keep the strip tension uniform and the edges burr-free; any burr can bridge adjacent turns and create inter-lamination shorts. If the wound core will be stress-relief annealed, the coating class must be compatible with the annealing temperature. Follow the recommendations of IEC 60404-8-7 and GB/T 2521.2 for grade designations and test methods, and ASTM A876 where US practice is required.
Common Mistakes
A frequent error is mixing strip widths from different suppliers, which produces cores with inconsistent stacking factor and uneven magnetic performance. Another is neglecting the rolling direction during core design; cutting the strip so that flux crosses the transverse direction can roughly double the core loss. Finally, moisture-damaged coils lose coating adhesion, so inspection of the coil ends on receipt is strongly recommended.
FAQ
What does the grade designation mean?
The letter indicates the grade family (for example Q for conventional, P for high induction, R for domain refined), and the number gives the guaranteed maximum core loss at 1.7 T/50 Hz in W/kg multiplied by 100. B23P090 therefore guarantees 0.90 W/kg at 1.7 T/50 Hz.
What is the difference between 0.23 mm and 0.30 mm strip?
Thinner strip has lower eddy-current loss but is more expensive and slightly reduces the lamination factor. For wound cores of small to medium rating, 0.27-0.30 mm is a common compromise; 0.23 mm is chosen for large power transformers where loss minimisation matters most.
Can slit coils be supplied in custom widths?
Yes. Widths are typically produced to order in the 30-120 mm range for wound-core work, with slitting tolerances held to a few tenths of a millimetre.
What coating classes are available?
Common options include inorganic and semi-organic insulating coatings with high insulation resistance; the choice depends on whether the core will be annealed after winding and on the operating temperature of the transformer.
How is core loss verified on delivery?
Loss is verified by Epstein frame testing per IEC 60404-2 or by ring-specimen measurement per IEC 60404-6, with certificates issued against the mill test report.