Material Basis of Cold Rolled Electrical Steel

Cold rolled electrical steel starts as a low-carbon silicon-iron alloy, hot rolled, cold rolled and finally annealed so that the recrystallised grains are randomly oriented. Random texture is the point: magnetic properties stay the same in every direction, which is what a rotating machine needs. Silicon content is usually 1.5-3.0 %, or silicon plus aluminium 1.8-4.0 %, and the product is normally supplied as fully processed strip in 0.35 mm and 0.50 mm nominal thickness, with 0.65 mm still common for heavier laminations.

Increasing silicon raises electrical resistivity and lowers eddy current loss, but it also lowers saturation induction and makes the strip harder and more brittle. Aluminium is therefore added to gain resistivity without taking silicon to an unworkable level. Impurities are held low: in the higher grades sulphur below 0.002 %, carbon below 0.003 %, nitrogen below 0.002 % and oxygen below 0.002 %, with titanium below 0.005 % and zirconium below 0.002 % to avoid fine carbonitride particles pinning grain growth.

How Grade Codes Encode Core Loss

Most commercial systems put the guaranteed loss into the grade name. Under EN 10106 the designation M400-50A means a non-oriented grade with maximum specific total loss of 4.00 W/kg at 1.5 T and 50 Hz in 0.50 mm thickness; M470-50A, M530-50A and M600-50A follow the same rule at 4.70, 5.30 and 6.00 W/kg. The GB/T 2521.1 designation works the same way in reverse order, so 50W470 is a 0.50 mm non-oriented grade at 4.70 W/kg and 35W300 is a 0.35 mm grade at 3.00 W/kg. JIS C 2552 and ASTM A677/A677M cover equivalent non-oriented fully processed products, and IEC 60404-8-4 is the parallel specification for the strip itself. Loss measurements are made on Epstein frames to IEC 60404-2, or on single sheets to IEC 60404-3.

Typical Property Ranges

Parameter Typical value Comment
Silicon content 1.5-3.0 % Si + Al 1.8-4.0 % in higher resistivity grades
Nominal thickness 0.35 mm, 0.50 mm, 0.65 mm 0.20-0.30 mm for high frequency machines
Specific total loss 2.30-8.00 W/kg at 1.5 T, 50 Hz Grade dependent, lower is better
Stacking factor 0.96-0.98 Depends on coating type and burr height
Insulation coating inorganic or inorganic plus organic Trades punchability against welding behaviour

Loss is quoted as total loss, meaning hysteresis plus eddy current components measured on a standard specimen. Because eddy loss grows with the square of thickness and frequency, a 0.35 mm grade always beats a 0.50 mm grade in the same loss class when the machine runs above line frequency.

Insulation Coatings and Stacking

The coating must insulate adjacent laminations, resist punching, take varnish and stay stable through the curing cycle of the machine. Thin inorganic coatings give the highest stacking factor and the best annealing behaviour; coatings with an organic addition improve punchability and die life but must be checked against the stress relief treatment, because some organic components do not survive the annealing temperature. Stacking factor, burr height, flatness and camber all show up directly in the stacking and in the loss of the finished core.

Applications and Selection

Non-oriented steel covers the whole rotating machine field: household motors and micromotors in the low-loss classes, industrial motors and generators in the medium and high silicon range, and traction motors in the thin-gauge, high-frequency classes. Ballasts, small transformers and magnetic switches are also typical. The practical selection rule is to set the grade by loss at the working frequency and induction, then check saturation induction for the flux the design needs, then confirm the coating system against the manufacturing route.

Frequently Asked Questions

Q: What does the number in a grade such as 50W470 mean?
A: In the GB/T 2521.1 system 50 is the nominal thickness in hundredths of a millimetre and 470 is the maximum specific total loss multiplied by 100, so the guarantee is 4.70 W/kg at 1.5 T and 50 Hz.

Q: Is cold rolled electrical steel the same as grain-oriented steel?
A: No. Cold rolled electrical steel here means the non-oriented product with random grain orientation for motors and generators, while grain-oriented strip is textured for unidirectional flux in transformer cores.

Q: Why are high-grade steels so low in carbon and sulphur?
A: Carbon causes magnetic ageing and sulphur and nitrogen form fine precipitates that pin grain boundaries; keeping them at the parts per million level allows large grains and low hysteresis loss.

Q: How much does aluminium help?
A: Aluminium raises resistivity like silicon and therefore lowers eddy current loss, but it also lowers saturation induction, so general grades hold aluminium at about 0.3-0.6 %.

Q: What thickness should be chosen for a 400 Hz machine?
A: Eddy loss scales with the square of frequency and thickness, so 0.20 mm and 0.35 mm grades are normally specified above 200 Hz instead of 0.50 mm.

Q: How is core loss checked on delivery?
A: Loss is verified on Epstein specimens to IEC 60404-2 or by single sheet tester to IEC 60404-3, as required by the material specification in IEC 60404-8-4.