What Is a Laminated Core: Structure, Materials and Manufacturing Process

Oct 17, 2025

Leave a message

A laminated core is a magnetic core built from a stack of thin electrical steel sheets that are insulated from one another. Almost every electric machine, from a household fan to the traction motor of an electric vehicle, contains such a stack, and the reason is simple: a solid steel core would allow large eddy currents to circulate, whereas a stack of insulated laminations interrupts those paths and cuts the resulting loss dramatically.

What a Laminated Core Is and Why It Is Laminated

When a conducting body sits in a changing magnetic field, eddy currents are induced in it and dissipate energy as heat. The induced voltage falls in proportion to the area enclosed by the current path, so dividing the core into thin sheets separated by insulation reduces the loss in roughly quadratic relation to the sheet thickness. That is why the magnetic circuit is built from laminations rather than one solid block.

Electrical steel strip, also called electrical sheet, is an iron-silicon alloy with specially controlled magnetic properties. Using it in laminated form gives the core low hysteresis loss, low eddy current loss and high permeability, which raises the efficiency of the machine and makes better use of the installed magnetic material.

Structure of a Lamination Stack

A motor stack is produced in two forms: the stator, which carries the winding, and the rotor, which turns inside it. Both are assembled from individual laminations of electrical steel insulated from each other.

Lamination thickness is normally between 0.10 mm and 1.00 mm; 0.35 mm, 0.50 mm and 0.65 mm have become the standard gauges.

Insulation is provided by a specific coating, typically only a few micrometres thick.

Shapes are produced by stamping for high-volume production or by laser cutting for prototypes and small to medium batches.

Laser cutting leaves almost no structural change at the cut edge compared with stamping, which can form a damaged zone with higher loss.

The finished stack is held together by interlocking, cleating, welding, adhesive bonding or the baking varnish process.

Cutting and Stacking Methods

With stamping, the individual sheets can be joined inside the punching tool itself, a process known as punch stacking. Laser-cut laminations are aligned in a fixture, stacked and then glued or baked. The baked varnish process and adhesive stacking both produce full-surface bonding, complete insulation between sheets and lower eddy current loss.

Full-surface bonding also suppresses vibration, improves heat conduction through the stack and allows filigree shapes to be assembled because no interlocking nibs or weld seams are needed. The trade-off is that the bonding step adds process time and requires a controlled baking cycle to cure the coating without damaging the magnetic properties of the steel.

Insulation Coatings

Various coatings are applied to the strip to prevent short circuits between laminations and to reduce eddy currents. Coating thickness generally varies from 1 to 4 micrometres, and the choice depends on the processing route and the final application.

Coating Main function Typical reason to select it
C3 Improves the lubricating effect Heavy punching and high-volume stamping
C4 Corrosion protection with insulation resistance General purpose cores exposed to humidity
C5 Optimises temperature resistance Stress-relief annealing after stamping
C6 Particularly high insulation resistance Large stacks and high-voltage equipment
Baking varnish Bonding technology for sheet packages Glued stacks with complete inter-lamination insulation

Material Selection

Electrical steel for laminated cores is an iron-silicon alloy and is divided into two families: non-grain-oriented (isotropic) steel and grain-oriented (anisotropic) steel. Non-oriented steel has almost uniform properties in every direction because the grains are randomly distributed, which suits rotating machines such as motors and generators. Grain-oriented steel is optimised along the rolling direction and is used in wound cores and stacked transformer cores where the flux follows that direction.

Type Example grade Nominal thickness Nominal core loss P1.7/50 Induction J800
Conventional grain oriented H23Q110 0.23 mm 1.10 W/kg 1.85 T
High permeability H23G085 0.23 mm 0.85 W/kg 1.90 T
Domain refined high permeability H23GK080 0.23 mm 0.80 W/kg 1.88 T

Typical lamination factors for these grades are in the range of 0.95 to 0.97, meaning that the stack consists of 95-97% steel and the remainder is coating and air. Core loss is guaranteed at a defined polarisation and frequency, so the grade must always be read together with its test condition.

Frequently Asked Questions

Q: Why are cores laminated instead of solid?
Because a solid conductive core would allow large eddy currents to circulate and convert energy into heat, while thin insulated laminations interrupt those paths and cut the loss sharply.

Q: Which lamination thickness should be used?
0.35 mm and 0.50 mm cover most motors and 0.65 mm is used in larger or low-cost designs; thinner gauges such as 0.10-0.20 mm are chosen for high-frequency applications where eddy current loss dominates.

Q: Is laser cutting better than punching?
Not universally. Punching is faster and cheaper for high volumes, while laser cutting gives design flexibility and a less damaged edge, which is an advantage for prototypes and for grades where edge loss matters.

Q: What is the difference between adhesive stacking and baking varnish?
Both bond the whole surface of each lamination. Adhesive stacking uses a glue layer applied during stacking, while the baking varnish process uses a coated strip that is cured in an oven after cutting.

Q: Which coating is used for annealing?
C5 is the coating selected when the stack is stress-relief annealed after stamping, because it is formulated to survive the annealing temperature without losing its insulation function.

Q: Can a laminated core be repaired if laminations short together?
Inter-lamination short circuits normally cannot be undone, so the coating quality, the burr height and the handling of the cut sheets during stacking are controlled from the start instead of corrected afterwards.

Send Inquiry