Amorphous C Core: Construction, Loss Behaviour and Selection for Power Electronics

Oct 16, 2025

Leave a message

What an Amorphous C Core Is

An amorphous C core is a magnetic core built from thin ribbons of a non-crystalline metal alloy, wound into a rectangular or oval shape and cut into two halves so that a bobbin or coil can be inserted. The ribbon is produced by rapid solidification, cooling molten alloy at roughly a million degrees per second so that no crystalline lattice can form. Without grains, there are no grain boundaries, and without grain boundaries the energy normally lost to domain wall pinning largely disappears. The result is very low core loss together with a modest saturation flux density.

The cut faces are usually lapped and clamped back together with a stainless or alloy band and resin, because the mating faces determine the effective air gap of the finished assembly. Gap control is the single largest influence on inductance tolerance in a gapped C core.

Why Magnetostriction and Loss Matter at High Frequency

In switched-mode conversion the core sees a unipolar or bipolar excitation at tens or hundreds of kilohertz. Loss then splits into hysteresis, eddy current and excess components, and eddy current loss rises with the square of frequency and with the square of ribbon thickness. Amorphous ribbon is typically supplied in the 20 to 30 micrometre range, far thinner than the 0.23 to 0.35 mm sheet used for grain-oriented electrical steel, so the eddy current term stays small over a much wider frequency band.

The trade-off is saturation flux density. Iron-based amorphous alloy saturates at about 1.56 T, against roughly 1.9 to 2.0 T for grain-oriented silicon steel. A designer therefore needs a larger core cross-section for the same flux, but gains lower temperature rise and lower loss per kilogram in return.

Parameter Amorphous ribbon core Grain-oriented silicon steel MnZn ferrite
Saturation flux density About 1.56 T About 1.9 to 2.0 T Roughly 0.4 T at 100 degrees C
Ribbon or sheet thickness About 20 to 30 micrometres 0.23 to 0.35 mm Bulk ceramic body
Curie temperature About 400 degrees C Above 700 degrees C Material dependent
Typical use band 50 Hz to about 100 kHz 50 to 400 Hz 20 kHz to several MHz

Construction Types and Gap Control

Uncut toroidal windings are not possible with brittle amorphous ribbon, which is why the C and U formats dominate. Three variants are common in production: resin-impregnated cores for low mechanical stress, clamped cores with a controlled gap for energy storage in inductors, and potted cores where the winding is fully encapsulated for environmental protection. In each case the finished inductance depends on the number of turns squared, the core cross-section, the mean magnetic path length and the effective permeability, which is dominated by the physical gap.

Because the effective permeability is often only a few tens of times higher than that of air when a gap is introduced, inductance becomes largely independent of the alloy temperature coefficient. That predictability is one reason amorphous C cores are used in current-mode chokes and in power factor correction inductors where stable inductance over temperature is more valuable than maximum permeability.

Application Areas in Power Electronics

The main uses are reactors, chokes, inverter output filters, medium-frequency transformer links and energy storage inductors in converters. Photovoltaic inverter DC links, electric vehicle on-board chargers, welding power supplies and uninterruptible power supply conversion stages all benefit from a core that stays cool at 20 kHz and above while carrying a significant bias current.

For line-frequency work, amorphous material is usually selected for its very low no-load loss rather than for its flux capability. In distribution applications the savings come from reduced no-load loss during the many hours a transformer spends lightly loaded, so the payback is a lifetime energy calculation rather than a first-cost comparison.

Specifying and Testing an Amorphous C Core

A complete specification should define the alloy family, ribbon thickness, build width and stack height, the cut gap, the mating face flatness, the banding or clamping method, and the acceptance limits for inductance and loss. Magnetic measurements on ring specimens are covered by IEC 60404-6 for the frequency range from 20 Hz to 200 kHz, while electrical steel measurement methods are defined in IEC 60404-2 for the Epstein frame and IEC 60404-3 for the single-sheet tester. Reactor and inductor test requirements are addressed in IEC 60076-6.

In practice, three checks catch most supplier problems: inductance at the rated bias current, core loss at a fixed flux density and frequency, and mechanical inspection of the mating faces for chipping or resin contamination. A core that meets inductance at zero bias but drifts under load usually has a gap problem rather than an alloy problem.

Frequently Asked Questions

Q: Why are amorphous cores always cut into C or U shapes?
A: The ribbon is thin, hard and brittle, so it cannot be wound through a coil the way a toroidal core is produced. Cutting the wound block into two halves allows the coil to be placed on the core and the magnetic circuit to be closed again with a controlled mating face.

Q: How does the cut gap affect inductance?
A: The gap dominates the effective permeability once it is introduced. Increasing the gap lowers effective permeability and reduces inductance, but it also raises the saturation current and stabilises inductance against temperature change, which is why gapped cores are used for energy storage inductors.

Q: Can an amorphous core replace a ferrite core at 100 kHz?
A: Sometimes. Amorphous ribbon has a much higher saturation flux density than ferrite, which helps with bias current, but ferrite still wins on loss at very high frequency and on core shapes available for small signal filtering. The crossover depends on flux level, frequency and allowable temperature rise.

Q: What causes high core loss in a finished C core?
A: Excess clamping pressure, damaged mating faces, resin penetration between laminations, or ribbon that was stressed during winding. Amorphous material is sensitive to mechanical stress because it is magnetostrictive, so a core that was fine before banding can show increased loss afterwards.

Q: How should loss be measured on an amorphous core?
A: Ring specimens are measured under IEC 60404-6, which defines the method for magnetically soft metallic and powder materials from 20 Hz to 200 kHz. Loss must always be stated together with flux density, frequency and temperature, because none of those values is meaningful alone.

Q: Is amorphous material suitable for line-frequency distribution transformers?
A: Yes, and it is widely used for that purpose. The advantage is a low no-load loss, which matters because no-load loss accrues continuously. The cost is a larger core cross-section because saturation flux density is lower than that of grain-oriented silicon steel.