Low Loss Nanocrystalline Toroidal Core for Transformer and Inductor Duty

Oct 14, 2025

Leave a message

What a Nanocrystalline Toroidal Core Is

A nanocrystalline toroidal core is a ring-shaped magnetic component wound from a very thin ribbon of an iron-based nanocrystalline alloy. The ribbon is rapidly solidified, so its grains are only nanometres across, which produces a combination of high permeability, low coercivity and low loss that sits between grain-oriented silicon steel and the higher-cost nickel-iron alloys. The ring form keeps the magnetic path short and closed and, because there is no air gap, leakage flux is very low.

Why the Material Is Used

Three properties drive the choice. First, permeability is very high, so a given inductance can be reached with far fewer turns of copper than a comparable ferrite or powdered-iron design, which shrinks the winding window and the component footprint. Second, saturation induction of about 1.2 T is roughly three times that of ferrite, so the core does not saturate under transient load steps. Third, the ribbon is only about 0.02 mm to 0.03 mm thick, which pushes eddy current loss low enough for use up to tens of kilohertz. The trade-off against silicon steel is cost and a lower saturation induction, and the trade-off against ferrite is a somewhat lower usable frequency ceiling.

Typical Properties at a Glance

Property Typical value Practical effect
Ribbon thickness 0.02 - 0.03 mm Low eddy current loss at medium frequency
Saturation induction About 1.2 T Core stays linear during load transients
Coercivity Low, typically below 1 A/m on annealed ribbon Narrow hysteresis loop, low residual loss
Operating temperature range Minus 55 degrees C to plus 120 degrees C Stable accuracy over wide ambient swings
Curie temperature About 570 degrees C No loss of properties at normal service temperatures
Magnetostriction Very low Minimal audible hum in the finished component

Core Sizes and DC Overcurrent Classes

The table lists representative toroidal core sizes together with the matched protective box, the effective cross-sectional area, the magnetic path length and the maximum DC overcurrent class, which is the direct current the core withstands while still meeting its accuracy requirement.

Core ID x OD x HT (mm) Box ID x OD x HT (mm) Effective area Ae (mm2) Magnetic path length Ie (mm) Max DC overcurrent class (A)
14 x 19 x 6.5 12 x 22 x 8 11.86 51.81 20
14 x 20 x 10 12 x 22.3 x 11.4 29.68 52.29 40
16 x 23 x 8 15 x 24 x 9.7 20.44 61.23 60
18 x 23 x 10 16.4 x 24.4 x 12.3 29.78 60.38 70
20 x 25 x 10 18.5 x 26.3 x 12.3 39.29 70.32 90
22 x 32 x 10 20.5 x 33.4 x 12.3 43.58 73.43 120
23 x 32 x 10 21.3 x 33.4 x 12.3 44.56 74.56 120

Applications in Power Electronics and Measurement

Common mode chokes are the largest application: a nanocrystalline ring with two opposed windings presents high impedance to common mode noise and low impedance to differential current, which is what an EMC filter needs to meet the conducted emission limits of CISPR 11 and CISPR 32. Current transformers take advantage of the high permeability to achieve a compact core with a small phase error, in accuracy classes defined by IEC 61869-2. Power factor correction inductors and boost chokes use the material where a compact footprint matters. Pulse transformers use it for waveform fidelity, and residual current circuit breakers use specially selected cores to detect small leakage currents without nuisance tripping.

Measurement and Quality Control

Magnetic properties of ring and toroidal cores are measured in accordance with IEC 60404-6 and ASTM A927/A927M, using a wound test winding and a defined excitation waveform. Because the measured inductance and loss depend on the test frequency, the number of turns and the flux density, the data sheet must state all three. Production controls that affect the result are ribbon thickness, winding tension, the annealing cycle that develops the nanocrystalline structure, casting into the protective box and the final winding of the customer's turns. Cutting a core to open it destroys the closed magnetic path and must be avoided.

Frequently Asked Questions

Q: What is the difference between a nanocrystalline and an amorphous core?
A: Both are rapidly solidified ribbons. Nanocrystalline ribbon is annealed to precipitate nanometre-scale grains, which gives much higher permeability and lower loss than amorphous ribbon at a higher cost.

Q: What is the saturation induction of a nanocrystalline core?
A: About 1.2 T, which is roughly three times that of a ferrite core but below the 1.8 T to 1.9 T induction available from grain-oriented silicon steel.

Q: Why does the toroidal shape reduce noise?
A: The closed ring geometry and the low magnetostriction of the material limit dimensional change during magnetisation, so far less audible hum is generated.

Q: Can a nanocrystalline core be used for a current transformer?
A: Yes. High permeability gives low excitation current and small phase error, so compact cores can reach the lower metering accuracy classes defined in IEC 61869-2.

Q: What does the DC overcurrent class in the size table indicate?
A: The direct current the core withstands while still meeting its accuracy specification, which is the key figure for residual current devices and DC-tolerant sensing.

Q: How should a nanocrystalline core be handled during assembly?
A: Keep the winding closed and protected by the box. Any cut through the ribbon breaks the magnetic path and permanently degrades permeability and accuracy.

Send Inquiry