Amorphous Toroidal Cores for Efficient Power Supply Magnetics
Oct 14, 2025
Leave a message
Amorphous toroidal cores are wound from thin, rapidly solidified metal ribbon into a closed ring. Because the ribbon is quenched far too quickly for a crystal lattice to form, the core contains no crystalline magnetic anisotropy, which gives it very high permeability together with a narrow hysteresis loop. Designers of switch-mode power supplies, uninterruptible power systems, inverters and adjustable-speed drives use these cores to build smaller, lighter and cooler magnetics at the same power rating.
How the Amorphous Structure Changes Core Behaviour
Amorphous alloy is cast from the melt directly into ribbon only about 20 to 30 micrometres thick. That single casting step replaces the rolling and annealing route used for conventional silicon steel, so the finished material has no grain boundaries and no easy axis of magnetisation. Reversing magnetisation therefore costs very little energy and the resulting B-H loop is almost free of hysteresis. In practice the structure delivers four benefits:
High permeability across the medium and high frequency range, comparable with premium ferrite grades.
Very low hysteresis loss, because domain walls are not pinned by grain boundaries.
Low eddy-current loss, because the ultra-thin ribbon limits the circulation of induced currents.
Stable usable performance from roughly 8 kHz to 100 kHz, the band in which power inductors and SMPS chokes normally operate.
Saturation Flux Density and Power Density
The decisive figure is saturation flux density. Ferrite cores typically saturate near 0.49 T, whereas amorphous metal can be driven to approximately 1.56 T before saturation. A core with more than three times the usable flux swing stores far more energy in the same volume, so either the toroid can be made smaller for a given inductance, or a given toroid can carry a much higher current before it saturates.
| Property | Amorphous metal toroid | Ferrite toroid |
|---|---|---|
| Saturation flux density | Approximately 1.56 T | Approximately 0.49 T |
| Dominant loss behaviour | Very low hysteresis loss, low eddy-current loss | Moderate hysteresis loss, low eddy-current loss |
| Typical working band | 8 kHz to 100 kHz | Frequently above 100 kHz |
| High-current capability | High, thanks to the large usable flux swing | Lower, because saturation is reached earlier |
Loss Behaviour Under Real Operating Conditions
Because an amorphous core responds readily to an alternating field, the hysteresis component of core loss stays low across the whole working band. Eddy-current loss, the second contributor, is governed by ribbon thickness: thinner ribbon means shorter current paths and less circulating current, so amorphous ribbon avoids the penalty that thicker laminations suffer as frequency rises. Together the two effects explain why an amorphous toroid usually runs cooler than a comparable silicon steel or powdered iron core, and why it can be pushed to a higher switching frequency without a thermal penalty. Where a substantial DC bias is superimposed, as in a filter choke, the peak flux should still be held well below saturation so that inductance is preserved and loss does not rise steeply.
Toroidal Core and Protective Box Dimensions
The table below lists representative amorphous ring cores together with their matching protective boxes, the effective cross-sectional area Ae, the magnetic path length Ie and the maximum DC overcurrent class. The range covers small filter cores through to large high-current chokes.
| Magnetic core size (mm) | Protective box size (mm) | Ae (mm2) | Ie (mm) | Max DC overcurrent class (A) | ||||
|---|---|---|---|---|---|---|---|---|
| id | od | ht | ID | OD | HT | |||
| 14 | 19 | 6.5 | 12 | 22 | 8 | 11.86 | 51.81 | 20 |
| 14 | 20 | 10 | 12 | 22.3 | 11.4 | 29.68 | 52.29 | 40 |
| 16 | 21 | 10 | 15 | 24 | 12.3 | 24.85 | 57.41 | 60 |
| 16 | 23 | 8 | 15 | 24 | 9.7 | 20.44 | 61.23 | 60 |
| 17 | 23 | 10 | 15.3 | 24.4 | 12.3 | 26.89 | 61.34 | 60 |
| 18 | 23 | 10 | 16.4 | 24.4 | 12.3 | 29.78 | 60.38 | 70 |
| 19 | 25 | 10 | 17.3 | 26 | 12.3 | 39.42 | 62.31 | 80 |
| 20 | 25 | 10 | 18.5 | 26.3 | 12.3 | 39.29 | 70.32 | 90 |
| 21 | 28 | 10 | 18.3 | 30 | 12.3 | 50.39 | 77.45 | 100 |
| 22 | 32 | 10 | 20.5 | 33.4 | 12.3 | 43.58 | 73.43 | 120 |
| 23 | 32 | 10 | 21.3 | 33.4 | 12.3 | 44.56 | 74.56 | 120 |
Selection and Design Checklist
Start from the inductance the choke must hold at full DC bias, then choose the smallest core whose Ae and Ie deliver that value with margin.
Compare the maximum DC overcurrent class with the worst-case fault current in the circuit, not only with the nominal load.
Check that the protective box inner diameter still clears the finished winding, since the wound core grows in outer and inner dimensions.
Budget the temperature rise: keep the working flux below saturation and derate the loss allowance accordingly.
Match the core to the switching frequency band; amorphous toroids give the greatest advantage between 8 kHz and 100 kHz.
Quality Control Points Before Assembly
Incoming inspection should confirm the dimensional tolerances of id, od and ht against the drawing, measure core loss on a representative sample at the specified frequency and flux, and check the integrity of the protective box and its coating. A measured inductance-versus-DC-bias curve is the most useful single record, because it shows whether the core still holds the required inductance at the current the design actually sees. Cores that are cut or gapped should be inspected for burrs and for consistent mating faces, since a poor joint raises loss and reduces effective permeability.
Frequently Asked Questions
Q: Why is an amorphous toroidal core more efficient than a ferrite core?
Its saturation flux density is approximately 1.56 T compared with about 0.49 T for ferrite, and its hysteresis loss is very low because the metal has no crystalline anisotropy, so more energy is stored with less loss in the same volume.
Q: Which frequency range suits amorphous toroidal cores best?
They are most advantageous between roughly 8 kHz and 100 kHz, where the combination of a large flux swing and low core loss outperforms silicon steel, ferrite and powdered iron alternatives.
Q: How does the thin ribbon reduce loss at high frequency?
Eddy currents circulate within the conductive material, and a ribbon only 20 to 30 micrometres thick greatly shortens those paths, so the eddy-current contribution to core loss is limited as frequency rises.
Q: Can an amorphous core be used in a DC-biased filter choke?
Yes, provided the peak flux with bias is kept well below the saturation level. The large usable flux swing leaves useful headroom, but inductance still falls as the core approaches saturation.
Q: What do Ae and Ie mean in the specification table?
Ae is the effective cross-sectional area of the magnetic path and Ie is its effective length. Both are needed to convert the material permeability into the inductance of a wound core.
Q: Does the protective box affect performance?
The box protects the brittle wound core and sets the space available for the winding, so it does not change the magnetic properties but it does constrain the copper cross-section and therefore the achievable current density.