Customized Nanocrystalline EI-Type Cores for Transformers and Inductors

Sep 24, 2025

Leave a message

An EI type nanocrystalline core is a magnetic component built from a rapidly solidified iron-based ribbon and formed into the classic E and I profile. The EI geometry puts the winding in an easy, bobbin-friendly window, while the nanocrystalline ribbon delivers very high initial permeability, high saturation induction and exceptionally low loss at the switching frequencies used by modern power electronics.

For designers of switched mode supplies, power factor correction stages and filter inductors, that combination means fewer turns, a smaller core and a lower temperature rise than a ferrite or laminated silicon steel part of the same rating. Sizes and stack heights can be produced to the winding window that is actually available on the board.

What a Nanocrystalline EI Core Is

The ribbon begins as an iron-based alloy containing silicon, boron, niobium and copper, melt spun into a strip only a few hundredths of a millimetre thick. In the as-cast state its structure is amorphous; a controlled heat treatment then crystallizes it into grains of roughly ten nanometres, which is where the name nanocrystalline comes from. That structure holds domain wall movement in check, so permeability rises, coercivity falls and high-frequency loss drops sharply compared with conventional crystalline alloys of similar saturation.

The ribbon is then wound or stacked into E and I shapes, bonded, cut to the required air gap and finish annealed, so the finished core holds a tight dimensional tolerance and stable magnetic values batch to batch.

Magnetic Features That Matter

High initial permeability - a given inductance needs fewer turns, so copper loss and winding volume fall.

High saturation magnetic induction - the core keeps working under surge current instead of saturating early.

Ultra-low high-frequency loss - the thin, resistive ribbon keeps eddy loss small at switching frequencies.

Excellent temperature stability - permeability and loss change little across the working range of power equipment.

Good DC bias resistance - inductance holds up when a DC component is superimposed, as in power factor correction and filter chokes.

Characteristic Typical value
Ribbon thickness 0.018–0.025 mm
Saturation induction about 1.2 T
Initial permeability tens of thousands, set by the heat treatment
Curie temperature above 500 °C
Useful frequency band 50 Hz to several hundred kHz

Standard EI Dimensions and Custom Sizes

EI cores are described by four dimensions: A is the overall length of the E, B its height, C the width of the centre limb and D the window width on each side. Common tooling sizes, in millimetres, are listed below.

A B C D
14 8.75 3.5 3.5
16 12 4 2
19 12.5 5 2.5
28 21 8 4
30 20 10 5
33 22 11 5.5
35 23.4 11.6 5.84
48 32 16 8
60 40 20 10
84 56 28 14
96 64 32 16
132 88 44 22

Sizes from a 14 mm to a 132 mm A dimension cover most board-level and industrial work. Intermediate sizes, taller stacks, gapped or ungapped assemblies and clamped constructions are produced to drawing.

Where EI Cores Are Used

Typical duties include switching power supply transformers, isolation transformers, rectifier transformers, common mode and differential inductors, power factor correction inductors, filter inductors and choke inductors. In each case the EI shape gives an accessible bobbin, generous creepage distance between primary and secondary, and a magnetic circuit whose air gap can be fixed precisely when the design needs to store energy rather than transfer it.

Customization and Quality Control

Item Option
Core profile standard EI, gapped EI, ungapped EI, cut core
Ribbon thickness 0.018 mm, 0.020 mm, 0.025 mm
Finish bare ribbon, resin impregnated, encapsulated in a protective case
Dimensional tolerance held to the agreed drawing, including the air gap where specified
Testing inductance, loss and dimensional checks on finished cores

Assembly practice matters as much as the ribbon itself. Cut faces are deburred so the mating E and I halves close cleanly, bobbin and core are matched in height, and the gap is set mechanically rather than left to the finish of the cut.

Frequently Asked Questions

Q: Why choose nanocrystalline ribbon instead of ferrite?
Saturation induction of about 1.2 T is far above that of ferrite, so the core is much smaller for the same power handling, and it tolerates a superimposed DC component without collapsing inductance.

Q: Are sizes other than the standard EI tooling available?
Yes. The standard range runs from a 14 mm to a 132 mm A dimension, and intermediate dimensions, stack heights and window proportions are produced to drawing.

Q: What is the air gap for?
Inductors that store energy, such as power factor correction and filter chokes, need a gap to stay linear under DC bias. Transformer cores are normally supplied ungapped.

Q: How thick is the ribbon and why does it matter?
Ribbon is normally 0.018 mm to 0.025 mm. A thin strip raises electrical resistance and shortens the eddy current path, which is what keeps loss low as switching frequency rises.

Q: Can a matched bobbin be supplied with the core?
Yes. Core, bobbin and clamping hardware are produced as a matched set so the winding window, creepage distances and assembly height are fixed before the board layout is released.

Q: What data is needed to specify a nanocrystalline EI core?
The four core dimensions, stack height, required air gap, target inductance, working current including any DC bias, switching frequency and insulation class.

Send Inquiry