B23R085 Silicon Steel for Laminated Transformer Cores: Grade, Loss and Build
Oct 22, 2025
Leave a message
The Grade Behind the Name
B23R085 is a cold-rolled grain-oriented electrical steel supplied in the fully processed state. The designation is decoded in three parts: 23 is the nominal thickness in hundredths of a millimetre, so the sheet is 0.23 mm thick; R identifies the regular grain-oriented type, as distinct from the high-permeability P type; and 085 states the maximum specific total loss as 0.85 W/kg at the reference condition of 1.7 T and 50 Hz. Grades in this family are specified in IEC 60404-8-7 and EN 10107, with ASTM A876 covering equivalent fully processed flat-rolled grain-oriented material.
The material is produced with a Goss texture, in which the easy magnetisation axis of most grains lies along the rolling direction. That texture is why a grain-oriented lamination must be laid with its rolling direction parallel to the flux path in the core; rotating a lamination by 90 degrees raises the loss dramatically. Loss and induction are verified on Epstein specimens under IEC 60404-2 or with a single sheet tester under IEC 60404-3.
Why Laminations, Not Solid Iron
A solid iron core would carry large eddy currents induced by the alternating flux, and the resulting circulation would convert a substantial share of the input power into heat. Laminating the core with thin, individually insulated sheets interrupts those circulating paths and confines each eddy current to a single sheet of 0.23 mm, which reduces the loss by roughly two orders of magnitude compared with a solid block of the same mass.
| Element of the build | Function | Typical practice |
|---|---|---|
| Silicon steel sheet | high permeability and high resistivity magnetic path | 0.23 mm grain-oriented strip, about 3 percent silicon |
| Insulating coating | prevents interlamination current | thin glass film plus insulation coating, a few micrometres |
| Lamination pattern | reduces joint reluctance | step-lap or mitred joints rather than butt joints |
| Clamping and impregnation | holds the stack rigid, limits noise and fretting | uniform pressure, resin or varnish where specified |
Core loss has two parts. Hysteresis loss depends on the material and on the flux density and frequency, and it cannot be reduced by laminating because it arises from the energy needed to move domain walls. Eddy-current loss depends on thickness, resistivity and frequency, and it is the part that laminating and thin strip address. At 50 Hz, moving from 0.35 mm to 0.23 mm strip cuts the eddy-current component by more than half, which is why thin grades are used in low-loss distribution transformers and in cores that run at elevated flux density.
Building the Laminated Core
The quality of the finished core depends more on the build than on the strip itself, because a good grade poorly stacked performs worse than a moderate grade stacked well.
Cut with sharp tooling, keep burr height low and never deburr by grinding, which smears metal across the insulation.
Keep the rolling direction aligned with the flux path in every limb and yoke.
Use a step-lap joint, so that only one lamination in each group of five or more is interrupted at any cross section.
Control stacking pressure; excessive clamp force raises loss and can damage the coating.
Keep the stack flat and clean. Oil, swarf and moisture between laminations destroy interlaminar resistance.
For cores that will be wound with aluminium or copper, the window and the limb dimensions must be held to a tight tolerance so the coil former is not distorted when the core is closed. A gap that is too large at the joint raises no-load current and audible noise, while a core that is too large for the coil is forced into place under stress, which raises loss.
Testing, Handling and Storage
Incoming checks on strip include thickness, coating thickness, specified loss and induction at the reference condition, plus a flatness and burr inspection. Finished cores are normally tested for core loss by the wattmeter method and for no-load current at rated voltage, and the results are compared with the design figure rather than with the strip certificate, because stacking and clamping raise loss by a few percent.
Grain-oriented strip is sensitive to mechanical stress and to corrosion. Store coils horizontally on a flat support, keep packs dry, and avoid stacking heavy items on cut laminations. Moisture is particularly damaging because surface rust destroys insulation resistance and contaminates transformer oil; where cores are stored for long periods, wrapping and desiccant protection are worth the cost. Once the core has been annealed and clamped, it should not be re-stacked or re-clamped without re-testing, since every handling step costs a small amount of performance.
Selection Guidance
Choose a regular grain-oriented grade such as B23R085 when the core operates at power frequency with a fixed flux direction and a modest loss budget. Choose a high-permeability grade when the target loss is tighter or when the design needs higher induction at a given magnetising field, and consider a 0.27 mm grade instead when tooling cost and stacking effort outweigh the last few watts of loss. In every case the decision should be made on measured loss of the finished core at the design flux density, not on the nominal strip figure alone.
Frequently Asked Questions
Q: What does the R in B23R085 mean?
A: The R denotes the regular grain-oriented type, as opposed to the high-permeability P type, and it tells the buyer which guarantee level to expect from the strip at the reference condition.
Q: What is the loss limit implied by B23R085?
A: The final three digits give the maximum specific total loss of 0.85 W/kg measured at 1.7 T and 50 Hz, with the measurement made on Epstein specimens under IEC 60404-2 or by the single sheet tester method of IEC 60404-3.
Q: Why must laminations be stacked with the rolling direction along the flux path?
A: Grain-oriented steel has its easy magnetisation axis in the rolling direction, so a lamination rotated away from that direction shows much higher loss and lower permeability, which would defeat the purpose of buying a grain-oriented grade.
Q: Does a thinner lamination always give lower loss?
A: It lowers the eddy-current component, which scales with the square of thickness, but hysteresis loss per kilogram does not fall and handling becomes more difficult, so the benefit is limited and is weighed against stacking cost and tooling wear.
Q: How much does the stacking process add to core loss?
A: A few percent is normal, arising from burrs, clamping stress and imperfect joints. That is why the guarantee is normally made on the finished core or with an explicit margin above the strip certificate value.
Q: Can a laminated core be repaired if a few laminations are damaged?
A: Limited local damage can be tolerated if the affected sheets are replaced and the stack re-clamped, but the core must be re-tested, because a shorted or burred region raises loss out of proportion to the small area it occupies.