1K107 High-Permeability Fe-Based Nanocrystalline Block Cores: Properties and Applications

Oct 28, 2025

Leave a message

What Is a 1K107 Fe-Based Nanocrystalline Core?

1K107 is a grade designation for a high-permeability Fe-based nanocrystalline alloy. The material is produced by rapidly quenching molten alloy into a ribbon roughly 25 μm thick, which is then wound or stacked and annealed under a magnetic field to develop a fine structure of nanoscale crystallites embedded in an amorphous matrix. This microstructure combines a high saturation magnetic induction of about 1.25 T with high permeability, low coercivity, and very low core loss at high frequencies, making 1K107 suitable for magnetic components that operate between roughly 20 kHz and 30 kHz and above.

Block Core Construction

A block core (also called a stacked block core) is built by stacking nanocrystalline ribbon segments or by flattening and pressing wound ribbons into a rectangular block shape, so that the magnetic path has a larger effective cross-section than a single toroid. The block form is then assembled with the required air gap or left gapless depending on the application. Because the annealed ribbon is brittle and sensitive to mechanical stress, the core is usually encapsulated or clamped with soft pressure distribution, and the stacking factor (the ratio of effective magnetic steel area to the geometric cross-section) is typically above 0.75 for this material class.

Key Magnetic and Physical Properties of 1K107

Property Typical Value Note
Saturation magnetic induction Bs ≈ 1.25 T higher than ferrite
Initial permeability μi high, ≥ 30,000 depends on annealing
Maximum permeability μmax very high, ≥ 100,000 field-annealed
Coercivity Hc low, ≤ 1 A/m soft magnetic behavior
Curie temperature ≈ 560°C good thermal stability
Saturation magnetostriction < 2×10⁻⁶ low noise
Resistivity ≈ 130 μΩ·cm limits eddy currents
Ribbon thickness ≈ 25 μm typical
Stacking factor > 0.75 block form
Operating frequency 20 kHz to 30 kHz and above application dependent

The combination of high saturation induction and low loss means that a 1K107 core can handle higher flux density than ferrite at the same frequency, which translates into a smaller core cross-section for a given power throughput.

Comparison with Other Core Materials

Compared with ferrite, 1K107 offers roughly double the saturation flux density, which reduces the turns count or core size in high-frequency transformers. Compared with amorphous ribbon, the nanocrystalline alloy provides higher permeability and lower core loss in the 20 kHz to 100 kHz range, although the material cost is higher. Compared with grain-oriented silicon steel, the nanocrystalline material has far lower loss at high frequency, but a lower saturation induction (about 1.25 T versus 1.7 T to 2.0 T) and a lower stacking factor, so silicon steel remains the choice for line-frequency power transformers.

Typical Applications

High-frequency power transformers for switch-mode power supplies operating at 20 kHz to 30 kHz.

Output filter inductors and EMI filter chokes of solar inverters.

Power factor correction (PFC) chokes in industrial and telecom power supplies.

Common-mode chokes and current transformers for precision measurement.

Magnetic amplifiers and pulse transformers where high permeability and fast response are required.

Design and Handling Considerations

Because the annealed nanocrystalline ribbon is brittle, block cores must be handled with care: avoid sharp impacts, do not exceed the recommended clamping pressure, and use a protective case where vibration is present. The effective area used in design calculations must include the stacking factor. In high-frequency applications, the winding layout should minimize leakage inductance and proximity-effect losses, and the core loss should be evaluated at the actual operating flux density and frequency, not at the material test condition, because loss rises steeply with both.

FAQ

Can a 1K107 block core replace a ferrite core in the same transformer?

Frequently yes, with a redesign. The higher saturation induction allows a smaller core or fewer turns, but the winding must be re-optimized because the core loss and copper loss balance changes.

What is the operating temperature range?

The material is stable up to the Curie temperature of about 560°C, far above any practical transformer temperature. The practical limit is set by the winding insulation and encapsulation material, typically 120°C to 180°C.

Why is the stacking factor lower than that of silicon steel?

The ribbon surface and the block assembly process leave small air spaces between layers; 0.75 to 0.85 is a realistic range for nanocrystalline blocks, so the designer must use the effective area in flux calculations.

Is the core loss lower than amorphous alloy at 20 kHz?

In general yes for the same flux density, which is why nanocrystalline is preferred for high-frequency power conversion, while amorphous remains competitive at lower frequencies and for larger cores.

Does the core need an air gap for PFC choke applications?

For a choke carrying DC bias, a distributed or discrete air gap is normally required to prevent saturation; the high permeability of 1K107 otherwise saturates under a small DC current.

In summary, 1K107 Fe-based nanocrystalline block cores deliver high permeability, high saturation induction and low high-frequency loss, which makes them a strong candidate for 20 kHz to 30 kHz transformers, inverter filters and PFC chokes, provided the design accounts for stacking factor and mechanical handling constraints.

Send Inquiry